Properties
| Measurement |
Test Method |
Value (90 minute UV post-cured) |
Value (90 minute UV + 2 hours @ 80ºC thermal post-cured) |
| Hardness, Shore D |
ASTM D 2240 |
84 |
85 |
Flexural Modulus
Flexural Strength |
ASTM D 790 |
2,400 Mpa (340 KSI)
83 Mpa (12,000 PSI) |
2,300 Mpa (330 KSI)
83 Mpa (12,000 PSI) |
Tensile Modulus
Tensile Strength
Elongation at Break |
ASTM D 638 |
2,300 Mpa (330 KSI)
53 Mpa (7,700 PSI)
11% |
2,300 Mpa (330 KSI)
59 Mpa (8,500)
10% |
| Impact Strength, Notched Izod |
ASTM D 256 |
34 J/m (0.6 ft-lbs/in) |
34 J/m (0.6 ft-lbs/in) |
| Heat Deflection Temperature |
ASTM D 648 @66 PSI ASTM D 648@264 PSI |
63ºC (145ºF)
52ºC (126ºF) | 97ºC (207ºF) 76ºC (169ºF) |
| Glass Transition (Tg) |
DMA, E" peak |
70ºC (158ºF) |
72ºC (162ºF) |
| Density |
|
1.22 g/cm3 |
|